China · GB
S30110
GB/T 1220:2007 — Stainless steel bars
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionPhysical properties
vs. temperatureChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.15 | |||
| Cr | 16 | 18 | ||
| Mn | 2 | |||
| N | 0.1 | |||
| Ni | 6 | 8 | ||
| P | 0.045 | |||
| S | 0.03 | |||
| Si | 1 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| bars, Solution treated, <= 180 mm | ≥205 | ≥520 | ≥40 | ≥60 | HV ≤200 HBW; HRB;HR ≤90 HBW; HRB;HB ≤187 HBW; HRB |
Physical properties
20.0
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 193.00 | 500.00 | 0.73 | 7.93 |
Typical physical values
| Density | Elastic modulus | Poisson's ratio | Remarks |
|---|---|---|---|
| 7.61–8.10 | 190.00–215.00 | 0.27–0.30 | Typical material properties for stainless steel. These values are not taken from the standard; they are indicative and must not be used for design. |
| 7.86 | 190.00–210.00 | 0.27–0.30 | Material properties for low-carbon, high-alloy steel. These values are not taken from the standard; they are indicative and must not be used for design. |
Heat treatment
| Type | 3 | 4 |
|---|---|---|
| Heat-treatment process | Solution-treated | 1010℃~1150℃, Rapidly cooled |
Similar grades
| Grade | Region | System |
|---|---|---|
| 4319-301-00-I | International standard | ISO |
| X5CrNi17-7 | International standard | ISO |
| SA-240 S30100 | ASME | |
| SA-240 Type 301 | ASME | |
| S30100 | UNS | |
| 301 | SAE | |
| SUS 301 | JIS | |
| 1.4319 | EN | |
| 1.4310 | EN | |
| X5CrNi17-7 | EN | |
| X 10 CrNi 18 8 | EN | |
| X 12 CrNi 17 7 | SEW | |
| X 10 CrNi 18 8 | DIN | |
| X 12 CrNi 17 7 | DIN | |
| 1.4310 | DIN | |
| 1Cr17Ni7 | GB |