United States · AISI
AISI 201
ASTM A473:2009 — Standard Specification for Stainless Steel Forgings
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.15 | |||
| Cr | 16 | 18 | ||
| Mn | 5.5 | 7.5 | ||
| N | 0.25 | |||
| Ni | 3.5 | 5.5 | ||
| P | 0.06 | |||
| S | 0.03 | |||
| Si | 1 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| forgings, Heat treated | ≥205 | ≥515 | ≥40 |