European Union · EN

E 69 2 2NiMo

EN 757:1997 — EN 757

Chemical composition

wt% · log scale
0.010.1110C0.03 – 0.1Cr0.2Cu0.3Mn1.4Mo0.3 – 0.6Nb0.05Ni1.8 – 2.6P0.025S0.02V0.05
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥690 MPaTensile strength Rm760–960 MPaImpact energy Kv/Ku≥47 JElongation A≥17 %

Chemical composition

ElementminmaxSimilarRemarks
C0.030.1
Cr0.2
Cu0.3
Mn1.4
Mo0.30.6
Nb0.05
Ni1.82.6
P0.025
S0.02
V0.05

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
electrodes≥690 The lower yield (ReL) is used760–960≥17 Gauge length is equal to five times the test specimen≥47 Charpy V Notch (-20°C)

High/low temperature

Impact energy Kv/Ku (J)
ConditionTemperature ℃minRemarks
electrodes-2047Charpy V Notch