United States · ACI

CN7MS

-- — -

Chemical composition

wt% · log scale
0.010.1110100C0.07Cr18 – 20Cu1.5 – 2Mn1Mo2.5 – 3Ni22 – 25P0.04S0.03Si2.5 – 3.5
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥205 MPaTensile strength Rm≥485 MPaElongation A≥35 %

Chemical composition

ElementminmaxSimilarRemarks
C0.07
Cr1820
Cu1.52
Mn1
Mo2.53
Ni2225
P0.04
S0.03
Si2.53.5

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
castings≥205≥485≥35 Lo=50mm;Amin=8% in Lo=25mm