Chemical composition
wt% · log scale- min – max range
- typical value
Physical properties
vs. temperatureCreep properties
- 100.0h
- 1000.0h
Temperature °C · time at rupture
Chemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 1.2 | 1.4 | ||
| Cr | 27 | 30 | ||
| Mn | 0.5 | 1 | ||
| Mo | 0.5 | |||
| Ni | 1 | |||
| P | 0.035 | |||
| S | 0.03 | |||
| Si | 1 | 2.5 |
Physical properties
20.0
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 18.80 | 500.00 | 7.60 |
Typical physical values
| Density | Elastic modulus | Poisson's ratio | Remarks |
|---|---|---|---|
| 7.80 | 190.00–210.00 | 0.27–0.30 | Typical properties for high-carbon high-alloy steel. These values are not taken from the standard; they are indicative and must not be used for design. |
Creep
| Temperature ℃ | Time h | Rp1 | CRS |
|---|---|---|---|
| 600 | 10000.0h | 26.0 | |
| 700 | 10000.0h | 11.0 | |
| 800 | 100.0h | 12.0 | |
| 800 | 1000.0h | 11.0 | |
| 800 | 10000.0h | 5.0 | |
| 900 | 100.0h | 7.0 | |
| 900 | 1000.0h | 5.0 | |
| 900 | 10000.0h | 1.5 |
Similar grades
| Grade | Region | System |
|---|---|---|
| 1.4777 | UNI | |
| GX130CrSi29 | UNI | |
| 1.4777 | UNE | |
| GX130CrSi29 | UNE | |
| 1.4777 | STAS | |
| GX130CrSi29 | STAS | |
| GX130CrSi29 | SS | |
| 1.4777 | SNV | |
| GX130CrSi29 | SNV | |
| 1.4777 | SFS | |
| GX130CrSi29 | SFS | |
| 1.4777 | PN | |
| GX130CrSi29 | PN | |
| 1.4777 | ONORM | |
| GX130CrSi29 | ONORM | |
| 1.4777 | NS | |
| GX130CrSi29 | NS | |
| 1.4777 | NBN | |
| GX130CrSi29 | NBN | |
| 1.4777 | MSZ | |
| GX130CrSi29 | MSZ | |
| 1.4777 | Czech Republic | CSN |
| GX130CrSi29 | Czech Republic | CSN |
| 1.4777 | Bulgaria | BDS |
| GX130CrSi29 | Bulgaria | BDS |
| 1.4777 | B.S. | |
| GX130CrSi29 | B.S. | |
| 1.4777 | AFNOR NF | |
| GX130CrSi29 | AFNOR NF | |
| GX130CrSi29 | DIN | |
| 1.4777 | DIN |