Hungary · MSZ
E 42 5 Mo
MSZ EN 499:1994 — MSZ EN 499
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| Cr | 0.2 | |||
| Cu | 0.3 | |||
| Mn | 1.4 | |||
| Mo | 0.3 | 0.6 | ||
| Nb | 0.05 | |||
| Ni | 0.3 | |||
| V | 0.05 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| Electrodes, deposited metal, welded condition | ≤420 | ≤500 | ≤20 | ≤47 |
High/low temperature
| Condition | Temperature ℃ | min | max |
|---|---|---|---|
| Electrodes | deposited metal as-welded | -50 | 47 |