Global · Enterprise standard
CARBODUR 20 MnCr 5
UNS
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.17 | 0.22 | ||
| Cr | 1 | 1.3 | ||
| Mn | 1.1 | 1.4 | ||
| P | 0.035 | |||
| S | 0.035 | |||
| Si | 0.4 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| soft annealed | HB ≤217 | |||||
| annealed to obtain spheroidal carbides | HB ≤180 | |||||
| Ferrite -pearlitic structure treated | HB 152–201 For diameters up to 60 mm |