Global · Enterprise standard

Erdemir 1325

-- — -

Chemical composition

wt% · log scale
0.010.1110C0.17Mn1P0.03S0.03Si0.1
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2250.00Tensile strength Rm330.00Elongation A19.00coil, heavy plate, sheet, strip, cold rolledYield strength Rp0.2250.00Tensile strength Rm330.00Elongation A17.00coil, steel strip, cold rolled, t <= 0.7 mm, heavy plate, sheet

Chemical composition

ElementminmaxSimilarRemarks
C0.17
Mn1
P0.03
S0.03
Si0.1

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
coil, heavy plate, sheet, strip, cold rolled250.00330.0019.00
coil, steel strip, cold rolled, t <= 0.7 mm, heavy plate, sheet250.00330.0017.00