Global · Enterprise standard

Erdemir 2105

-- — -

Chemical composition

wt% · log scale
0.0010.010.11Al0.02 – 0.07C0.04 – 0.08Mn0.2 – 0.35N0.008P0.02S0.02Si0.025
  • min – max range
  • typical value

Mechanical properties

value range by condition
HardnessPlatecoil, steel strip, , annealed, 0.21 mm < t <= 0.28 mm, HR, sheetYield strength Rp0.2225.00Tensile strength Rm325.00coil, steel strip, , annealed, 0.21 mm < t <= 0.28 mm, heavy plate, sheetHardnessPlatecoil, steel strip, , annealed, t <= 0.21 mm, HR, sheetYield strength Rp0.2225.00Tensile strength Rm325.00coil, steel strip, , annealed, t <= 0.21 mm, heavy plate, sheet

Chemical composition

ElementminmaxSimilarRemarks
Al0.020.07
C0.040.08
Mn0.20.35
N0.008
P0.02
S0.02
Si0.025

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
coil, steel strip, , annealed, 0.21 mm < t <= 0.28 mm, HR, sheetPlate 53.00
coil, steel strip, , annealed, 0.21 mm < t <= 0.28 mm, heavy plate, sheet225.00325.00
coil, steel strip, , annealed, t <= 0.21 mm, HR, sheetPlate 54.00
coil, steel strip, , annealed, t <= 0.21 mm, heavy plate, sheet225.00325.00
coil, steel strip, , annealed, t > 0.28 mm, HR, sheetPlate 52.00
coil, steel strip, , annealed, t > 0.28 mm, heavy plate, sheet225.00325.00