Chemical composition
wt% · log scale- min – max range
- typical value
Chemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.6 | 0.7 | ||
| Cr | 0.25 | For L limits;0.3% max for H limits;1.4% max for antigraphitization | ||
| Cr+Ni+Cu+Mo | 0.8 | When one or more of these elements is specified | ||
| Cu | 0.3 | For L limits;0.5% max for H limits | ||
| Mn | 0.6 | 0.9 | ||
| Mo | 0.1 | For L limits;0.16% max for H limits | ||
| Ni | 0.3 | For both limits | ||
| P | 0.03 | |||
| S | 0.035 | |||
| Si | 0.15 | 0.3 | For Type 1;0.1% max for Type 2 |