Sweden · SS

A2-80

SS EN ISO 3506-2

Chemical composition

wt% · log scale
0.010.1110100C0.1Cr15 – 20Cu4Mn2Ni8 – 19P0.05S0.03Si1
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥800 MPa

Chemical composition

ElementminmaxSimilarRemarks
C0.1For steel having a max. C content of 0.03%
Cr1520If Cr is below 17%
Cu4
Mn2
Ni819
P0.05
S0.03
Si1

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
nuts≥800