FE-PA3601

SS EN 2573

Chemical composition

wt% · log scale
0.010.1110100C0.08Cr17 – 19Mn2Ni9 – 12P0.045S0.03Si1Ti0.7
  • min – max range
  • typical value

Mechanical properties

value range by condition
Tensile strength Rm≤780 MPaElongation A≥40 %

Physical properties

vs. temperature
Elastic modulus GPa
165 – 200°C
Mean thermal expansion 10⁻⁶/K
16.0 – 18.0°C

Chemical composition

ElementminmaxSimilarRemarks
C0.08
Cr1719
Mn2
Ni912
P0.045
S0.03
Si1
Ti0.7>= 5 x %C

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
Wires, , > 0.25 <= 3 mm≤780≥40

Physical properties

20.0

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
200.0015.00500.000.737.90

Fatigue

Test conditions
ItemDetail
ProductSemi Finished products; Thickness: <= 450 mm; Quenched
ExperimentReversed bending; T: 20°C
Specimen
Monotonic
PropertyValue
Yield strength (MPa)190.0
Tensile strength (MPa)500.0 700.0
Elongation (%)30.0
Stress life
No.Cycles
11E7

Similar grades

GradeRegionSystem
4541-321-00-IInternational standardISO
SA-813 S32100United StatesASME
FE-PA3601ItalyUNI
FE-PA3601SpainUNE
FE-PA3601RomaniaSTAS
FE-PA3601SwitzerlandSNV
FE-PA3601FinlandSFS
FE-PA3601PolandPN
FE-PA3601AustriaONORM
FE-PA3601NorwayNS
FE-PA3601BelgiumNBN
FE-PA3601HungaryMSZ
FE-PA3601GermanyDIN
FE-PA3601Czech RepublicCSN
FE-PA3601BulgariaBDS
FE-PA3601United KingdomB.S.
FE-PA3601FranceAFNOR NF
SA-403 S32100United StatesASME
SA-403 WP 321United StatesASME
A182 F 321United StatesASTM
SA-813 TP321United StatesASME
SA-182 F 321United StatesASME