China · GB

ML06Cr12Nb

GB/T 4232:2009 — Stainless steel wire for cold heading and cold forging

Chemical composition

wt% · log scale
0.010.1110100C0.08Cr10.5 – 12.5Mn1Nb1Ni0.5P0.04S0.03Si1
  • min – max range
  • typical value

Mechanical properties

value range by condition
Tensile strength Rm≤650 MPaReduction of area Z≥55 %Wires, , 0.8 < d <= 3.0 mmTensile strength Rm≤650 MPaElongation A≥10 %Reduction of area Z≥55 %Wires, , 3.0 < d <= 20.0 mm

Chemical composition

ElementminmaxSimilarRemarks
C0.08
Cr10.512.5
Mn1
Nb1%Nb= 6 x %C
Ni0.5
P0.04
S0.03
Si1

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
Wires, , 0.8 < d <= 3.0 mm≤650≥55
Wires, , 3.0 < d <= 20.0 mm≤650≥10≥55