China · CGMA

17Cr2Ni2MoH

CGMA001-1:2004 — CGMA001-1

Chemical composition

wt% · log scale
0.0010.010.1110C0.15 – 0.19Cr1.5 – 1.8Cu0.2Mn0.4 – 0.6Mo0.25 – 0.35Ni1.4 – 1.7P0.03S0.015 – 0.035Si0.15 – 0.4
  • min – max range
  • typical value

Mechanical properties

value range by condition
Impact energy Kv/Ku≥63 Jsteel productsHardnessHRHardnessHRHardnessHRHardnessHRsteel products, normalized 910±10℃, quenched 830±10℃HardnessHBsteel products, annealed or tempered

Chemical composition

ElementminmaxSimilarRemarks
C0.150.19
Cr1.51.8
Cu0.2
Mn0.40.6
Mo0.250.35
Ni1.41.7
P0.03
S0.0150.035
Si0.150.4

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
steel products≥63
steel products, normalized 910±10℃, quenched 830±10℃HR 30–37 End hardenability,J50;HR 34–41 End hardenability,J25;HR 39–46 End hardenability,J10;HR 41–47 End hardenability,J5
steel products, annealed or temperedHB ≤217

Heat treatment

Type34
Heat-treatment processTemperedHeating temperature 200℃, water coolant, air
Heat-treatment processQuenchedHeating temperature 870℃, oil coolant
Heat-treatment processNormalizedHeating temperature 930℃