China · Wugang Q/WTB

A516-65

WJX 061:2010 — WJX 061

Chemical composition

wt% · log scale
0.010.1110C0.29C0.29C0.28C0.26C0.24Mn0.79 – 1.3Mn0.79 – 1.3P0.03S0.02Si0.13 – 0.45
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥240 MPaTensile strength Rm450–585 MPaElongation A≥23 %Elongation A≥19 %

Chemical composition

ElementminmaxSimilarRemarks
C0.29Thickness >200mm
C0.29Thickness >100~200mm
C0.28Thickness >50~100mm
C0.26Thickness >12.5~50mm
C0.24Thickness ≤12.5mm
Mn0.791.3Thickness >12.5mm
Mn0.791.3Thickness ≤12.5mm
P0.03
S0.02
Si0.130.45

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
steel plates, normalized≥240450–585≥23 Lo = 50mm;≥19 Lo = 200mm

High/low temperature

Impact energy Kv/Ku (J)
ConditionTemperature ℃min
steel plates normalized027