Germany · DIN
Sint-C 01
DIN 30910-4:2004 — Sintered metal materials - Sintered-material specifications - Part 4: Materials for structural parts
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.3 | 0.9 | ||
| Cu | 1 | |||
| Fe | Bal | |||
| Other | 2 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| Condition not stated | ≥170 Rp 0.1% | ≥240 | ≥2 Breaking tension | HB ≥75 Permissible hardness is minimum 70 HB |
Physical properties
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 100.00 |
Similar grades
| Grade | Region | System |
|---|---|---|
| Sint-D 01 | DIN |