Japan · JIS
SMS 2035
JIS Z2550:2000 — Sintered metal materials-Specification
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.2 | |||
| Cr | 12 | 14 | ||
| Fe | Balance | |||
| Total others | 3 | Refer to P |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| powder metallurgy products, sintered | ≥350 | ≥1 |
Physical properties
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 6.80 |
Similar grades
| Grade | Region | System |
|---|---|---|
| SMS 2025 | JIS |