NIONICRAL-70

-- — -

Chemical composition

wt% · log scale
0.0010.010.1110C0.13Ce0.59Cr1.15Mn0.3Ni2.8P0.015S0.015Si0.3
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2680–690 MPaTensile strength Rm740–940 MPaImpact energy Kv/Ku≥118 JElongation A≥16 %

Chemical composition

ElementminmaxSimilarRemarks
C0.13
Ce0.59
Cr1.15
Mn0.3
Ni2.8
P0.015
S0.015
Si0.3

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
Plates, hot rolled, t = 16 mm680–690740–940≥16 L=5 mm≥118