European Union · EN
EN AW-5049
EN 754-2:2013 — Aluminium and aluminium alloys - Cold drawn rod/bar and tube - Part 2: Mechanical properties; German version EN 754-2:2013
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionPhysical properties
vs. temperatureChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| Al | Bal | |||
| Cr | 0.3 | |||
| Cu | 0.1 | |||
| Fe | 0.5 | |||
| Mg | 1.6 | 2.5 | ||
| Mn | 0.5 | 1.1 | ||
| Others each | 0.05 | Includes listed elements for which no specific limit is shown. | ||
| Si | 0.4 | |||
| Ti | 0.1 | |||
| Total Others | 0.15 | The sum of those "Others" metallic elements 0.010% or more each | ||
| Zn | 0.2 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| Drawn tubes, Annealed +O, <= 20 mm | ≥80 | 180–250 | ≥17 | HB ≥50 HBW (typical value) | ||
| Drawn tubes, Strain-hardened - 1/8 hard +H11, <= 17 mm | ≥100 | 195–260 | ≥13 | HB ≥58 HBW (typical value) | ||
| Drawn tubes, Strain-hardened - 3/4 hard +H16, <= 5 mm | ≥200 | 260–310 | ≥3 | HB ≥83 HBW (typical value) | ||
| Drawn tubes, Strain-hardened - 3/8 hard +H13, <= 12 mm | ≥140 | 225–280 | ≥7 | HB ≥70 HBW (typical value) | ||
| Drawn tubes, Strain-hardened - 4/4 hard +H18, <= 3 mm | ≥240 | ≥280 | ≥2 | |||
| Drawn tubes, Strain-hardened - 5/8 hard +H15, <= 7 mm | ≥180 | 250–300 | ≥3 | HB ≥80 HBW (typical value) | ||
| Drawn tubes, Strain-hardened - 7/8 hard +H17, <= 4 mm | ≥220 | 270–320 | ≥2 | HB ≥85 HBW (typical value) | ||
| Drawn tubes, Strain-hardened only +H111, <= 20 mm | ≥80 | 180–250 | ≥17 | HB ≥50 HBW (typical value) | ||
| Drawn tubes, strain hardened - 1/2 +H14, <= 10 mm | ≥160 | 240–290 | ≥4 | HB ≥75 HBW (typical value) | ||
| Drawn tubes, strain hardened - 1/4 +H12, <= 15 mm | ≥120 | 210–270 | ≥10 | HB ≥65 HBW (typical value) |
Physical properties
20.0
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 70.00 | 23.50 | 138.00 | 896.00 | 0.05 | 2.70 | 0.33 |
Typical physical values
| Density | Elastic modulus | Poisson's ratio | Remarks |
|---|---|---|---|
| 2.60–2.90 | 69.00–79.00 | 0.33 | Typical property values for aluminum alloys. These values are not taken from a published standard; they are indicative only and must not be used for design. |
Similar grades
| Grade | Region | System |
|---|---|---|
| 1050A | AA | |
| EN AW-AlMg2Mn0 | 8 | Italy |
| EN AW-5049 | UNI | |
| EN AW-AlMg2Mn0 | 8 | Spain |
| EN AW-5049 | UNE | |
| EN AW-AlMg2Mn0 | 8 | Sweden |
| EN AW-5049 | SS | |
| EN AW-AlMg2Mn0 | 8 | Switzerland |
| EN AW-5049 | SNV | |
| EN AW-AlMg2Mn0 | 8 | Finland |
| EN AW-5049 | SFS | |
| EN AW-AlMg2Mn0 | 8 | Poland |
| EN AW-5049 | PN | |
| EN AW-AlMg2Mn0 | 8 | Austria |
| EN AW-5049 | ONORM | |
| EN AW-AlMg2Mn0 | 8 | Norway |
| EN AW-5049 | NS | |
| EN AW-AlMg2Mn0 | 8 | Belgium |
| EN AW-5049 | NBN | |
| EN AW-AlMg2Mn0 | 8 | Hungary |
| EN AW-5049 | MSZ | |
| EN AW-AlMg2Mn0 | 8 | Germany |
| EN AW-5049 | DIN | |
| EN AW-AlMg2Mn0 | 8 | Czech Republic |
| EN AW-5049 | Czech Republic | CSN |
| EN AW-AlMg2Mn0 | 8 | United Kingdom |
| EN AW-5049 | B.S. | |
| EN AW-AlMg2Mn0 | 8 | Bulgaria |
| EN AW-5049 | Bulgaria | BDS |
| EN AW-AlMg2Mn0 | 8 | Romania |
| EN AW-5049 | ASRO | |
| EN AW-AlMg2Mn0 | 8 | France |
| EN AW-5049 | AFNOR NF | |
| 5049 | AA | |
| 3.3527 | DIN | |
| AlMg2Mn0 | 8 | Germany |