Japan · JIS
AC3A
JIS H5202:2010 — Copper alloy continuous castings
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| Al | Bal | |||
| Cr | 0.15 | |||
| Cu | 0.25 | |||
| Fe | 0.8 | |||
| Mg | 0.15 | |||
| Mn | 0.35 | |||
| Ni | 0.1 | |||
| Pb | 0.1 | |||
| Si | 10 | 13 | ||
| Sn | 0.1 | |||
| Ti | 0.2 | |||
| Zn | 0.3 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| Permanent mould castings +F | ≥170 | ≥5 | HB ≤50 Approx. HBW (for informative purposes and not specification value) | |||
| sand castings +F | ≥140 | ≥2 | HB ≤45 Approx. HBW (for informative purposes and not specification value) |