Germany · DIN
CuAl 5 As
DIN EN 12451 — Copper and copper alloys - Seamless, round tubes for heat exchangers; German version EN 12451:2012
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| Al | 4 | 6.5 | ||
| As | 0.1 | 0.4 | ||
| Cu | Bal | |||
| Fe | 0.2 | |||
| Mn | 0.2 | |||
| Ni | 0.2 | |||
| Other | These alloys may be used for applications in sea water | |||
| Pb | 0.02 | |||
| Sn | 0.05 | |||
| Total Others | 0.3 | |||
| Zn | 0.3 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| H075 | HV 75–110 | |||||
| R350 | ≥110 | ≥350 | ≥50 |
Physical properties
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 8.20 |
Similar grades
| Grade | Region | System |
|---|---|---|
| AlBz5 | DIN | |
| CW300G | UNI | |
| CuAl5As | UNI | |
| CW300G | UNE | |
| CuAl5As | UNE | |
| CW300G | SS | |
| CuAl5As | SS | |
| CW300G | SNV | |
| CuAl5As | SNV | |
| CW300G | SFS | |
| CuAl5As | SFS | |
| CW300G | PN | |
| CuAl5As | PN | |
| CW300G | ONORM | |
| CuAl5As | ONORM | |
| CW300G | NS | |
| CuAl5As | NS | |
| CW300G | NBN | |
| CuAl5As | NBN | |
| CW300G | MSZ | |
| CuAl5As | MSZ | |
| CW300G | DIN | |
| CW300G | Czech Republic | CSN |
| CuAl5As | Czech Republic | CSN |
| CW300G | B.S. | |
| CW300G | Bulgaria | BDS |
| CuAl5As | Bulgaria | BDS |
| CW300G | ASRO | |
| CuAl5As | ASRO | |
| CW300G | AFNOR NF | |
| CuAl5As | AFNOR NF | |
| CuAl5As | B.S. | |
| C60800 | UNS | |
| 2.0918 | DIN |