Germany · DIN

CuCo1Ni1Be

DIN EN 12420 — Copper and copper alloys - Forgings; German version EN 12420:1999

Chemical composition

wt% · log scale
0.1110Be0.4 – 0.7Co0.8 – 1.3Fe0.2Ni0.8 – 1.3Total Others0.5
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥500 MPaTensile strength Rm≥650 MPaElongation A≥8 %HardnessHVHardnessHB

Chemical composition

ElementminmaxSimilarRemarks
Be0.40.7
Co0.81.3
Cu​​Bal​​
Fe0.2
Ni0.81.3
Total Others0.5

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
Drop and hand forgings, H210≥500≥650≥8HV ≥220;HB ≥210

Physical properties

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
0.048.80

Similar grades

GradeRegionSystem
CW103CItalyUNI
CW103CSpainUNE
CuCo1Ni1BeSpainUNE
CW103CSwedenSS
CW103CSwitzerlandSNV
CuCo1Ni1BeSwitzerlandSNV
CW103CFinlandSFS
CuCo1Ni1BeFinlandSFS
CW103CPolandPN
CuCo1Ni1BePolandPN
CW103CAustriaONORM
CuCo1Ni1BeAustriaONORM
CW103CNorwayNS
CuCo1Ni1BeNorwayNS
CW103CBelgiumNBN
CuCo1Ni1BeBelgiumNBN
CW103CHungaryMSZ
CuCo1Ni1BeHungaryMSZ
CW103CGermanyDIN
CW103CCzech RepublicCSN
CuCo1Ni1BeCzech RepublicCSN
CW103CUnited KingdomB.S.
CW103CBulgariaBDS
CuCo1Ni1BeBulgariaBDS
CW103CRomaniaASRO
CuCo1Ni1BeRomaniaASRO
CW103CFranceAFNOR NF
CuCo1Ni1BeFranceAFNOR NF
CuCo1Ni1BeItalyUNI
CuCo1Ni1BeUnited KingdomB.S.
CuCo1Ni1BeSwedenSS