德国 · DIN

1.0413

DIN EN ISO 16120-2:2015 — 非合金钢线材转换线 - 第2部分:通用线材的具体要求

化学成分

元素minmax相似备注
Al0.01The value for Al can be fixed at 0.01% to 0.06%. In such cases the value of Si can be fixed at <=0.10% on request.The value for Al can be fixed at 0.01% to 0.06%. In such cases the value of Si can be fixed at <=0.10% on request.
C0.120.17Product analysis tolerance +/-0.02%Product analysis tolerance +/-0.02%
Cr0.2up to 0.30%up to 0.30%
Cu0.3A maximum Cu content of 0.20% may be agreed.A maximum Cu content of 0.20% may be agreed.
Mn0.30.6Product analysis tolerance +/-0.06%; Maximum not exceeding 1.20% and a minimum not lower than 0.30%.Product analysis tolerance +/-0.06%; Maximum not exceeding 1.20% and a minimum not lower than 0.30%.
Mo0.05
Ni0.25
P0.035Product analysis tolerance +0.005%Product analysis tolerance +0.005%
S0.035Product analysis tolerance +0.005%Product analysis tolerance +0.005%
Si0.3Product analysis tolerance +/-0.04%; For wire rod intended for galvanization the maximum Si level may be further restricted.Product analysis tolerance +/-0.04%; For wire rod intended for galvanization the maximum Si level may be further restricted.
V0.050.1