EN 4628:2013 — 航空航天系列 - 钢FE-PM3504(X4CrNiMo16-5-1) - 空气熔炼 - 淬火和回火 - 钢筋 - De = 150 mm - 1 100 MPa = Rm = 1 300 MPa

化学成分

元素minmax相似备注
C0.06
Cr1517
FeBaseBase
Mn1.5Where a higher strength is requiredWhere a higher strength is required
Mo0.81.5
N0.02
Ni46
P0.03
P+S0.023For specific welding applications and after agreement.For specific welding applications and after agreement.
S0.005
Si0.7

力学性能

热处理 / 状态屈服强度抗拉强度伸长率断面收缩率冲击功硬度
棒材 75 ≤ d-直径 ≤ 150mm   淬火及回火1150–1300 长-转≥8 长-转
棒材 75 ≤ d-直径 ≤ 150mm  淬火及回火≥900 长-转≥50 At -30℃;纵向;≥20 Charpy V Notch (120°C)HB 341–401 HBW;长-转
棒材 d-直径 ≤ 150mm   退火HB ≤293 HBW
棒材 d-直径 ≤ 75mm   hardened(direct quenching on hot rolled products) and temperedHB 341–401 HBW;纵向
棒材 d-直径 ≤ 75mm   hardened(direct quenching on hot rolled products) and tempered≥14 纵向
棒材 d-直径 ≤ 75mm  hardened(direct quenching on hot rolled products) and tempered≥900 纵向1150–1300 纵向≥100 Notch direction T;长-转;≥60 At -30℃;长-转

物理性能

20.0

弹性模量平均热膨胀系数热导率比热容电阻率密度泊松比
200.0015.00430.000.807.70

典型物理值

密度弹性模量泊松比备注
7.61–8.10190.00–215.000.27–0.30不锈钢的典型材料性能数值,此值不来源于标准,它是指示性指标,不能被用于设计用途。
7.86190.00–210.000.27–0.30低碳,高合金钢材料性能属性数值,此值不来源于标准,它是指示性指标,不能被用于设计用途。

相似牌号

牌号地区标准体系
4418-431-77-E国际标准ISO
FE-WM 3504欧盟EN
FE-PM 3504欧盟EN
1.4418意大利UNI
X 4 CrNiMo 16 5 1意大利UNI
1.4418西班牙UNE
X 4 CrNiMo 16 5 1西班牙UNE
1.4418罗马尼亚STAS
X 4 CrNiMo 16 5 1罗马尼亚STAS
1.4418瑞典SS
X 4 CrNiMo 16 5 1瑞典SS
1.4418瑞士SNV
X 4 CrNiMo 16 5 1瑞士SNV
1.4418芬兰SFS
X 4 CrNiMo 16 5 1芬兰SFS
1.4418波兰PN
X 4 CrNiMo 16 5 1波兰PN
1.4418奥地利ONORM
X 4 CrNiMo 16 5 1奥地利ONORM
1.4418挪威NS
X 4 CrNiMo 16 5 1挪威NS
1.4418比利时NBN
X 4 CrNiMo 16 5 1比利时NBN
1.4418匈牙利MSZ
X 4 CrNiMo 16 5 1匈牙利MSZ
1.4418捷克CSN
X 4 CrNiMo 16 5 1捷克CSN
1.4418保加利亚BDS
X 4 CrNiMo 16 5 1保加利亚BDS
1.4418英国B.S.
X 4 CrNiMo 16 5 1英国B.S.
1.4418法国AFNOR NF
Remanit 4418全球企业标准
415M全球企业标准
VIRGO 39全球企业标准
BÖHLER N404 EXTRA全球企业标准
X 4 CrNiMo 16 5 1法国AFNOR NF
1.4418欧盟EN
X 4 CrNiMo 16 5 1德国DIN
1.4418德国DIN